Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 105 kV/mm @Thickness 0.0762 mm |
2670 kV/in @Thickness 0.00300 in |
ASTM D149 |
Westlake Plastics ECTFE Film Made from HALAR® Ethylene-chlorotrifluoroethylene Resin Excellent purity. Excellent chemical resistance. Low permeability. Excellent abrasion resistance. Excellent temperature resistance.Halar® is a trade name of Solvay Solexis, Inc. Information p.. |