Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellamid® MRGF25/15 42H-WBK Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced, Weatherable Grade

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® MRGF25/15 42H-WBK Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced, Weatherable Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BlackAll information provided by Wellman Engineered Resins.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
DIS 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.011 cm/cm
0.0070 - 0.011 in/in
DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 105 MPa
15200 psi
ISO 527-93
Elongation at Break 3.0 %
3.0 %
ISO 527-93
Flexural Strength 165 MPa
23900 psi
ISO 178-93
Flexural Modulus 9.50 GPa
1380 ksi
ISO 178-93
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-93
Users viewing this material also viewed the following: