UBE UMERIT 1500F Metallocene LLDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer UBE
Trade Name UMERIT
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE UMERIT 1500F Metallocene LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical properties by being able to acquire any targeted molecular structures. Specific Notes for this Grade: UMERIT® 1500F offers various excellent properties: Superior low temperature seal property, advantageous compared to 2000F, Reduced motor load at processing, Draw resonance at high-speed drawing hardly occursInformation provided by UBE.
Physical Properties Metric English Comments
Density 0.913 g/cc
0.0330 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 1000 hour
1000 hour
F50; ASTM D1693
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
ASTM D2240
Tensile Strength, Yield 39.0 MPa
5660 psi
ASTM D638
Elongation at Break 730 %
730 %
ASTM D638
Tensile Modulus 0.190 GPa
27.6 ksi
Bending Modulus; ASTM D790
Thermal Properties Metric English Comments
Melting Point 99.0 °C
210 °F
UBE method
Vicat Softening Point 97.0 °C
207 °F
ASTM D1525