Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
M. Holland Company MAGMA® LM112-K LLDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ExxonMobil Method |
ExxonMobil LD 509.48 Compounding Resin
(discontinued **) LD 509.48 is a high melt index homopolymer resin designed to provide good processability in compounding applications.Information provided by ExxonMobil Chemical |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | Yield Density |
Honeywell PMP Polymethylpentene Film
(discontinued **) PMP is a clear, red, or blue film manufactured from polymethylpentene. It provides more toughness and heat resistance than standard polyolefins for release film applications.Information provided by.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5023 400 Micron LDPE Powder Description: ICOFLO 510-5023 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5056 500 Micron LDPE Powder Description: ICOFLO 510-5056 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5057 80 Micron LDPE Powder Description: ICOFLO 510-5057 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5058 1200 Micron LDPE Powder Description: ICOFLO 510-5058 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5062 500 Micron LDPE Powder Description: ICOFLO 510-5062 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5063 800 Micron LDPE Powder Description: ICOFLO 510-5063 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5019 300 Micron LDPE Powder Description: ICOTEX 520-5019 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a .. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5056 500 Micron LDPE Powder Description: ICOTEX 520-5056 is a low density polyethylene powder that has been developed to meet the special requirement of the textile coating industry. Key Characteristics: very high flow, very g.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5062 500 Micron LDPE Powder Description: ICOTEX 520-5062 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: very high melt flow, .. |
|||
Density | 0.913 g/cc @Temperature 121 °C |
0.0330 lb/in³ @Temperature 250 °F |
Dry Density |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M44 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Density | 0.913 - 0.919 g/cc | 0.0330 - 0.0332 lb/in³ | ASTM D4883 |
Westlake Epolene® C-17 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer Product Description: Epolene C-17 is a branched low density polyethylene with a relatively high melt point and viscosity compared to other Epolene C-type Polymers. It is useful to modify paraffin wa.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
UBE UMERIT 1500F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
UBE UMERIT 1520F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D1505 |
UBE UMERIT 613A Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM D792 |
Ensinger TECAFINE™ PP Polypropylene (PP) TECAFINE™ PP is an anti-stated, polypropylene, random copolymer polyolefin engineering plastic providing excellent chemical resistance and high purity. FDA compliant with better mechanical propert.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 654 Low Density Polyethylene Resin (European Grade) Product Description: LD 654 is a very high flow LDPE grade with a very good flexibility. It can be added to low-flowing LDPE grades to improve their processability.Availability: Africa & Middle East.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 655 Low Density Polyethylene Resin (European Grade) Product Description: LD 655 is a very high flow LDPE grade with a very good flexibility. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabiliz.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | |
Dow AFFINITY™ SM 1350 Polyolefin Plastomer AFFINITY® SM 1350 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in durable injection molded housewares and compression molded closure liners or gaskets. It exhibit.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | |
Dow ATTANE™ 4301 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4301 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It has low levels of sli.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | |
Dow ATTANE™ 4501 Ultra Low Density Polyethylene, Blown Film Grade ATTANE® 4501 copolymer is an ultra low density polyethylene having high tear strength and impact resistance, designed for use in industrial/ consumer film applications, either as a high performance.. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | |
Dow ATTANE™ 4701 Ultra Low Density Polyethylene, Medical Packaging Grade ATTANE® 4701 copolymer is an ultra low density polyethylene having high pinhole and puncture resistance, tear strength and high impact resistance combined with improved softness. It has low levels .. |
|||
Density | 0.913 g/cc | 0.0330 lb/in³ | ASTM C134 |
BNZ Materials BNZ-26 HS Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.913 - 1.19 g/cc | 0.0330 - 0.0430 lb/in³ | Average value: 0.940 g/cc Grade Count:29 |
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Masterbatch Grade". Each property range of values reported is minimum a.. |
|||
Density | 0.913 - 0.945 g/cc | 0.0330 - 0.0341 lb/in³ | Average value: 0.935 g/cc Grade Count:49 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report.. |