Trelleborg R525 Commercial Natural Rubber Polyisoprene

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Trelleborg
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg R525 Commercial Natural Rubber Polyisoprene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All information provided by Trelleborg
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Tensile Strength, Yield 8.00 MPa
1160 psi
Elongation at Break 400 %
400 %
Tear Strength 20.0 kN/m
114 pli
Compression Set 38 %

@Temperature 70.0 °C,
Time 79200 sec
38 %

@Temperature 158 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Descriptive Properties Value Comments
Color Red