Trelleborg Commercial Neoprene® C798 Chloroprene

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Trelleborg
Trade Name Commercial Neoprene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Commercial Neoprene® C798 Chloroprene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grades over 60° Shore A.Good resistance to heat, ozone and weathering.Flame retardant grades available.Good adhesion to metal.Resistance to chemicals; resistant to inorganic chemical products, except oxidizing acids and halogens. Moderate resistance to aliphatic hydrocarbons.All information provided by Trelleborg
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength, Yield 4.00 MPa
580 psi
Elongation at Break 200 %
200 %
Tear Strength 12.0 kN/m
68.5 pli
Compression Set 43 %

@Temperature 70.0 °C,
Time 79200 sec
43 %

@Temperature 158 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
Minimum Service Temperature, Air -25.0 °C
-13.0 °F
Descriptive Properties Value Comments
Color Black