Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tra-Con Tra-Duct 916H02 Room Temperature Cure, Conductive Silver Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Electrically Conductive , Filled/Reinforced Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Duct
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Duct 916H02 Room Temperature Cure, Conductive Silver Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-DUCT 916H02 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical properties. This two-part, smooth paste formulation of refined pure silver and epoxy is free of solvents and copper or carbon additives. It develops strong, durable, electrically and thermally conducting bonds and coatings between many different and dissimilar materials such as metals, ceramics, glass and plastic laminates. TRA-DUCT 916H02 cures at room temperature and can be used as a cold solder for heat-sensitive components where hot-soldering is impractical. It also can be used for the assembly and repair of electrical modules, printed circuits, wave guides, flat cables and high frequency shields. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 14000 cP

@Temperature 25.0 °C
14000 cP

@Temperature 77.0 °F
Mixed (cp #52, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 89
89
72 hrs @ 25°C
90
90
1 hr @ 65°C
Adhesive Bond Strength 7.72 MPa
1120 psi
Lap shear, alum to alum, 72 hrs @ 25°C
11.0 MPa
1590 psi
Lap shear, alum to alum, 1 hr @ 65°C
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 71.0 °C
160 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 0.010 ohm-cm
0.010 ohm-cm
cured 1 hr @ 65°C
0.010 ohm-cm
0.010 ohm-cm
cured 72 hrs @ 25°C
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
4320 min

@Temperature 25.0 °C
72.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Amber
Hardener
Silver
Cured
Mix Ratio, parts by weight 100/6
Resin/Hardener
Thixotropic Index 2.3
1 rpm/10 rpm
Working Life hours 1