Johnson Matthey Matti-sil 30 Cadmium Free Brazing Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Johnson Matthey
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey Matti-sil 30 Cadmium Free Brazing Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The wide melting range of Matti-sil 30 makes it suitable for filling larger joint gaps and producing fillets where desired.Optimum Joint Gap 0.075 - 0.2 mm.AWS A5.8-92 BAg-20Federal Specification QQ-B-564 BAg-20Equivalent to Engelhard Silvaloy A-30Equivalent to Handy & Harman Braze 300Equivalent to J W Harris Safety-Silv 30Information provided by Johnson Matthey.
Thermal Properties Metric English Comments
Melting Point 675 - 765 °C
1250 - 1410 °F
Solidus 675 °C
1250 °F
Liquidus 765 °C
1410 °F
Component Elements Properties Metric English Comments
Copper, Cu 38 %
38 %
Silver, Ag 30 %
30 %
Zinc, Zn 32 %
32 %