Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Toyobo ECOVYLOPET® EMC2330 PET Bottle Recycling Grade, 30% Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer Toyobo
Trade Name ECOVYLOPET®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toyobo ECOVYLOPET® EMC2330 PET Bottle Recycling Grade, 30% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: PET Bottle Recycling Grade, 30% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
Water Absorption 0.060 %
0.060 %
24 hrs at 23°C
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 2.00 mm
0.0030 in/in

@Thickness 0.0787 in
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
Tensile Strength at Break 142 MPa
20600 psi
Elongation at Break 2.2 %
2.2 %
Modulus of Elasticity 10.0 GPa
1450 ksi
Flexural Strength 195 MPa
28300 psi
Izod Impact, Notched 0.810 J/cm
1.52 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
0.455 MPa
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
Processing Properties Metric English Comments
Mold Temperature 110 °C
230 °F