Mechanical Properties Metric English Comments
Flexural Strength <= 195 MPa
<= 28300 psi
ISO 178
Polykemi AB SCANAMID 66 A12^ QF2515 Nylon 66,Mineral and Glass Fiber Reinforced
Information provided by Polykemi AB
Flexural Strength <= 195 MPa
<= 28300 psi
ISO 178
Polykemi AB SCANAMID 66 A13^ F15 Nylon 66, Glass Fiber Reinforced
Information provided by Polykemi AB
Flexural Strength 195 MPa
28300 psi
ISO 178/1A
Radici Raditer® B RVA 300 Polybutylene Terephthalate with 30% Glass fiber
Raditer® B RVA is a range of glass fiber reinforced Polybutylene terephthalate blends for injection molding, with excellent dimensional stability, low warpage and good surface aspect.Information pr..
Flexural Strength 195 MPa
28300 psi
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrically ..
Flexural Strength 195 MPa
28300 psi
Lehmann & Voss LUVOCOM® 20-7927 Polyphthalamide, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
Flexural Strength 195 MPa
28300 psi
Lehmann & Voss LUVOCOM® 3-7088-2 Polyamide 6, with carbon fiber and glass fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
Flexural Strength 195 MPa
28300 psi
ASTM D790
Gromax PBT 4130-201D 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Flexural Strength 195 MPa
28300 psi
Lehmann & Voss LUVOCOM® 1105-0779/WT PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High chemical resistance parts, hydrolysis resistance, non flammable.H..
Flexural Strength 195 MPa
28300 psi
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/BK PBT, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Flexural Strength 195 MPa
28300 psi
ISO 178
Solvay TECHNYLSTARâ„¢ S 216 V35 PA6, 35% glass filled, Conditioned
Description: TECHNYLSTAR polyamide, reinforced with 35% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North AmericaProduct Applications..
Flexural Strength 195 MPa
28300 psi
ASTM D 790
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC
LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supp..
Flexural Strength 195 MPa
28300 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® VX8532 PBT+PET (Europe-Africa-Middle East)
VALOX VX8532 is a 30% glassfiber reinforced, non blooming, flame retardant PBT+PET blend with excellent surface appearance and good ultrasonic weldability properties.This data was supplied by SABIC-..
Flexural Strength 195 MPa
28300 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON OEL13I PPS - Linear
LNP* STAT-KON* OEL13I is a compound based on PPS-Linear resin containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: High Impact, Wear Resistant, Electrically Conductive.
Flexural Strength 195 MPa
28300 psi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp HX05073 PA 11
LNP THERMOCOMP* HX05073 is a compound based on Nylon 11 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Strength 195 MPa
28300 psi
2.8% strain; ISO 178
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/HK060AE
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
Flexural Strength 195 MPa
28300 psi
ISO 178-93
Wellman Wellamid® GF1758-BK2 33% Glass Fiber Reinforced Nylon 66
Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman.
Flexural Strength 195 MPa
28300 psi
ASTM D790
Polyram RamTough PZ300G6 Polycarbonate, 30% Glass Fiber
30% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Flexural Strength 195 MPa
28300 psi
ASTM D790
Polyram RamTough RZ300G6 Polycarbonate, 30% Glass Fiber
30% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Flexural Strength 195 MPa
28300 psi
ISO 178
Polyram RamLloy PB917G6 Nylon 6/Polypropylene Alloy, 30% Glass Fiber Reinforced
30% Glass fiber reinforced Nylon6/PP alloy with reduced water absorption, dimensional stability and UV stabilized, for injection molding applications.Information provided by Polyram.
Flexural Strength 195 MPa
28300 psi
cond; ISO 178
DSM Novamid® 1015G35 NAT PA6-GF35
35% Glass Reinforced, Injection Molding
Flexural Strength 195 MPa
28300 psi
cond; ISO 178
DSM Novamid® 1015GH35 BK37 PA6-GF35
35% Glass Reinforced, Heat Stabilized, Injection Molding
Flexural Strength 195 MPa
28300 psi
ASTM D790
Ensinger Tecapeek® XP-119 Compression Molded PEEK Compound, 10% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Flexural Strength 195 MPa
28300 psi
ISO 178
Eurostar Star L PA6 30V D61 PA6, Glass Filled, Injection Molding
Star L PA6 30V D61 is a PTFE/Silicone Oil Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Flexural Strength 195 MPa
28300 psi
ISO 178
Eurostar Staramide RF004EU PA66/6, 20% Glass Fiber Filled, Injection Molded
Staramide RF004EU is a 20% Glass Fiber Reinforced Polyamide 66/6 Injection Molding (also known as Staramide 66C 20V S4)Information provided by Eurostar.
Flexural Strength <= 195 MPa
<= 28300 psi
ISO 178
Azoty Tarnow™ Tarnamid® T-27 CF10 Polyamide 6 10% Carbon Fiber - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
Flexural Strength 195 MPa
28300 psi
ISO Data
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin..
Flexural Strength 195 MPa
28300 psi
ASTM D790
Beijing Ranger Chem PBT-201-G30 211 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Flexural Strength 195 MPa
28300 psi
ISO 178
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Conditioned (2.5% Moisture)
Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..
Flexural Strength 195 MPa
28300 psi
ISO 178
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, Conditioned
Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..
Flexural Strength 195 MPa
28300 psi
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..