Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 3.45 MPa
>= 500 psi
ASTM D412
Multibase Multi-Flex® TPE A 6900 LC BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tensile Strength, Ultimate 3.45 MPa
500 psi
Across Flow; ASTM D412
ExxonMobil Vyram™ 9101-75 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Tensile Strength, Ultimate 3.45 MPa
500 psi
Loctite® Ultra Grey® 5999 Flange Sealant
Silicone GasketingLoctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing formulations for cure-in-place..
Tensile Strength, Ultimate 3.45 MPa
500 psi
Dymax 910 Strain Relief, Wire and Parts Tacking Adhesive
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 910 Strain Relief, Wire and Parts Tacking AdhesiveFlexible, good adhesion and mechanical removable Cure Type: UV
Tensile Strength, Ultimate 3.45 MPa
500 psi
Dymax 952 Potting and Encapsulation Adhesive
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 952 Potting and Encapsulation AdhesiveFast curing, high strength, flexible, excellent moisture resistance. Cure Typ..
Tensile Strength, Ultimate 3.45 MPa
500 psi
Bond strength to metal
Dymax Light Weld® 425 High Clarity Glass Bonding Adhesive
Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond..
Tensile Strength, Ultimate >= 3.45 MPa
>= 500 psi
ASTM C297
Touchstone CFOAM® 25 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..
Tensile Strength, Ultimate 3.45 MPa
500 psi
Across Flow; ASTM D412
ExxonMobil Vyram™ 9201-75 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
Tensile Strength, Ultimate 3.45 - 165 MPa
500 - 23900 psi
Average value: 95.5 MPa Grade Count:92
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..