Maximum Service Temperature, Inert 3000 °C
5430 °F
GrafTech GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material
GRAFOIL® GTA premium flexible graphite is a non-inhibited grade developed for use in nuclear or semiconductor applications. It is certified to meet the most rigorous purity specifications of the ..
Maximum Service Temperature, Inert 3000 °C
5430 °F
Destech Open-Celled Glassy Carbon Foam
Destech glassy (vitreous) carbon foam is available in different grades depending on the number of pores per inch (ppi). Standard grades are 10, 45, 100 and 500 ppi. Custom grades are available on a..
Maximum Service Temperature, Inert 3000 °C
5430 °F
Aremco AREMCOLOX™ 502-1600 (99%) Machinable Boron Nitride 99%
Hot-pressed high purity 99% boron nitride. High thermal conductivity. Easily machined. Non-reactive in molten salts, aluminum and other metals. Plates from 1/4" to 1" thick; rods from 1/4" to 3"..
Maximum Service Temperature, Inert 3000 °C
5430 °F
Touchstone CFOAM® 25 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..
Maximum Service Temperature, Inert >= 3000 °C
>= 5430 °F
Touchstone CFOAM® 30 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..
Maximum Service Temperature, Inert >= 3000 °C
>= 5430 °F
Touchstone CFOAM® 20 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..