Polymer Property : Electrical Resistivity = 0.0100 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0100 - 10000 ohm-cm
0.0100 - 10000 ohm-cm
NanoAmor 50% Regular Single Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, and gas-discharge tubes in telecom networksElectromagnetic-wave absorption an..
Electrical Resistivity 0.0100 - 10000 ohm-cm
0.0100 - 10000 ohm-cm
NanoAmor 95%, OD/ID: 20-40/5-10 nm Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Electrical Resistivity 0.0100 - 1.00e+16 ohm-cm
0.0100 - 1.00e+16 ohm-cm
Average value: 2.76e+15 ohm-cm Grade Count:79
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
Electrical Resistivity 0.0100 - 1.00e+12 ohm-cm
0.0100 - 1.00e+12 ohm-cm
Average value: 1.03e+10 ohm-cm Grade Count:59
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Electrical Resistivity 0.0100 - 100 ohm-cm
0.0100 - 100 ohm-cm
Average value: 22.6 ohm-cm Grade Count:9
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
Electrical Resistivity <= 0.0100 ohm-cm

@Temperature 65.6 - 150 °C
<= 0.0100 ohm-cm

@Temperature 150 - 302 °F
Average value: 0.00364 ohm-cm Grade Count:5
Overview of materials for Epoxy, Electrically Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of..
Electrical Resistivity <= 0.0100 ohm-cm

@Time 900 - 10800 sec
<= 0.0100 ohm-cm

@Time 0.250 - 3.00 hour
Average value: 0.00364 ohm-cm Grade Count:5
Overview of materials for Epoxy, Electrically Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of..
Electrical Resistivity 0.0100 - 200000 ohm-cm
0.0100 - 200000 ohm-cm
Average value: 13200 ohm-cm Grade Count:17
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Electrical Resistivity 0.0100 - 0.100 ohm-cm
0.0100 - 0.100 ohm-cm
Applied Coating; formulated with DMSO or MEG
Heraeus Cleviosâ„¢ P Conductive Sulfonate Polymer for Antistatic Coatings
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P is an antistatic material based on PEDOT:PSS..
Electrical Resistivity 0.0100 - 0.100 ohm-cm
0.0100 - 0.100 ohm-cm
Applied Coating; formulated with DMSO or MEG
Heraeus Cleviosâ„¢ PH Conductive Sulfonate Polymer for Antistatic Coatings
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PH is an antistatic material based on PEDOT:PS..
Electrical Resistivity 0.0100 ohm-cm
0.0100 ohm-cm
cured 24 hr at 25°C (77°F). Value is 0.003 Ohm-cm cured 3 hr at 65°C (150°F)
Von Roll Isola IMI E-Solder® 3022 Electrically Conductive Adhesive
Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t..
Electrical Resistivity 0.0100 ohm-cm
0.0100 ohm-cm
Von Roll Isola IMI E-Solder® 3026 Electrically Conductive Adhesive
Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t..
Electrical Resistivity 0.0100 - 1.00e+7 ohm-cm
0.0100 - 1.00e+7 ohm-cm
Tailorable; ASTM D4496
Touchstone CFOAM® 25 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..
Electrical Resistivity 0.0100 - 5.00e+14 ohm-cm
0.0100 - 5.00e+14 ohm-cm
Average value: 2.00e+14 ohm-cm Grade Count:4
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..