Total Finaclear® MBF Clear Impact Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finaclear® MBF Clear Impact Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The MBF masterbatch is a master batch especially developed for reducing blocking and denesting problems that can occur during the processing of Finaclear® modified GPPS on sheet extrusion and thermoforming lines. When blended with Finaclear® polymers and GPPS, the MBF masterbatch complies with most of the food regulations in European countries and with the Food and Drug Administration (FDA) in the USA.ApplicationThe MBF masterbatch is designed to be used with Finaclear® 520 modified GPPS as well as with Finaclear® 530 modified GPPS.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
ASTM D1895B
Density 1.04 g/cc
0.0376 lb/in³
Finaprene 2602 Method
Melt Index of Compound 16.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238G
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified