Material Notes:
FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmium free polyethylene specially developed for the manufacture of pressure pipes and fittings and accessories for gas distribution networks.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D 792
Viscosity 1.30e+6 cP

@Shear Rate 100 1/s,
Temperature 190 °C
1.30e+6 cP

@Shear Rate 100 1/s,
Temperature 374 °F
ATOFINA research test
Environmental Stress Crack Resistance >= 700 hour
>= 700 hour
ASTM D1693
Oxidative Induction Time (OIT) >= 20 min
>= 20 min
210°C; EN 728
>= 30 min
>= 30 min
200°C; EN 728
Melt Flow 0.20 g/10 min

@Load 2.16 kg
0.20 g/10 min

@Load 4.76 lb
ASTM D 1238
0.92 g/10 min

@Load 5.00 kg
0.92 g/10 min

@Load 11.0 lb
ASTM D 1238
High Load Melt Index 18 g/10 min

@Load 21.6 kg
18 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
DIN 53505
Tensile Strength at Break 32.0 MPa
4640 psi
ISO 527
Tensile Strength, Yield 18.0 MPa
2610 psi
ISO 527
Elongation at Break >= 700 %
>= 700 %
ISO R527
Elongation at Yield 9.0 %
9.0 %
ISO 527
Modulus of Elasticity 0.700 GPa
102 ksi
ISO 178
Flexural Modulus 0.700 GPa
102 ksi
ASTM D 790
Thermal Properties Metric English Comments
Heat of Fusion 160 J/g
68.8 BTU/lb
DSC
Specific Heat Capacity 2.00 J/g-°C
0.478 BTU/lb-°F
DSC
2.60 J/g-°C

@Temperature 150 °C
0.621 BTU/lb-°F

@Temperature 302 °F
DSC
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
DIN 52612
0.200 W/m-K

@Temperature 150 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 302 °F
DIN 52612
Melting Point 125 - 129 °C
257 - 264 °F
crystalline; DSC
Vicat Softening Point 125 °C
257 °F
ISO 306
Brittleness Temperature -100 °C
-148 °F
ASTM D 746
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
IEC 93
Surface Resistance >= 1.00e+16 ohm
>= 1.00e+16 ohm
IEC 93
Dielectric Constant 2.35

@Frequency 1000 Hz
2.35

@Frequency 1000 Hz
IEC 250
Dielectric Strength 16.0 kV/mm
406 kV/in
IEC 243
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
IEC 250