Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 16.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
16.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238G |
Total Finaclear® MBF Clear Impact Polystyrene