Tipco Tipcolene® FPT 40 NEX - 40% Talc Reinforced Polypropylene Homopolymer, Low MFI

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® FPT 40 NEX - 40% Talc Reinforced Polypropylene Homopolymer, Low MFI.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% Talc Reinforced PP HomopolymerApplications: Sheets, Pipes, ProfilesProcessing: ExtrusionInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Melt Flow <= 2.0 g/10 min
<= 2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Break >= 30 %
>= 30 %
ASTM D638
Flexural Yield Strength 51.5 MPa
7470 psi
ASTM D790
Flexural Modulus 4.40 GPa
638 ksi
ASTM D790
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
226 °F
ASTM D648