Material Notes:
Features: Homopolymer, Narrow Molecular Wt. Dist.Uses: Disposable Drinkware, Medical Applications, PackagingApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 22 g/10 min

@Load 2.16 kg,
Temperature 230 °C
22 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 35.2 MPa
5100 psi
2 in/min; ASTM D638
Elongation at Break 12 %
12 %
2 in/min; ASTM D638
Flexural Modulus 1.34 GPa
195 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
0.125 in; ASTM D256
Descriptive Properties Value Comments
Form Pellets