Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.62 MPa | 1250 psi | ASTM D412 |
Polymax® Maxelast® C4970 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Strength, Yield | 8.60 MPa | 1250 psi | ASTM D412 |
Precision Polymer Engineering F60R Fluorosilicone Rubber Red Fluorosilicone, 56-65 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 60.Applications: S.. |
|||
Tensile Strength, Yield | 8.60 MPa | 1250 psi | ASTM D412 |
Precision Polymer Engineering N90E Nitrile Rubber High Nitrile Rubber, 85-95 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR. Aerospace Material Specification DTD5509.. |
|||
Tensile Strength, Yield | 8.62 MPa | 1250 psi | ASTM D638 |
Multibase Multi-Flex® D 4201 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone Resistant General Purpose Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInformation p.. |
|||
Tensile Strength, Yield | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Flexalloy® 3501-45-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Tensile Strength, Yield | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex Flexalloy® 9100-45 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Tensile Strength, Yield | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex TEKRON® 4300-D90A Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex UNIPRENE® 7400-80 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.62 MPa | 1250 psi | 100% Retention, Hot Air Aging, 22 hrs at 70°C |
Teknor Apex UNIPRENE® 7400-80 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 8.62 MPa @Temperature 21.1 °C |
1250 psi @Temperature 70.0 °F |
Flatwise Tensile |
Hexcel® Redux® 312/5 Modified epoxy film adhesive Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support.. |
|||
Tensile Strength, Yield | 8.62 MPa | 1250 psi | ASTM D412 |
ACC EP AJS EPI Engineered Polymers Aliphatic Joint Sealant EP AJS Aliphatic Joint Sealant, “Powered by Reactamine® Technology, is a two component 100% solid, aliphatic (silicone optional) polyurea based joint sealant. EP AJS is a self-leveling joint seala.. |
|||
Tensile Strength, Yield | 8.62 MPa | 1250 psi | ASTM D-638 |
Axiall 14750 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 8.62 MPa | 1250 psi | ASTM D-638 |
Axiall 8552 Moldings & Extrusions Flexible PVC A soft extrusion compound recommended for profiles, weatherstrips and sheeting. Also suitable for injection molding.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201.. |
|||
Tensile Strength, Yield | 8.62 MPa | 1250 psi | ASTM D412 |
Teknor Apex APEX® 94-A0098C-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-ClearForms-PelletsProcessing Method-Injection Molding.. |