Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resin Technology Group TIGA 291-EX Grey Medium Viscosity Polyamide Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group TIGA 291-EX Grey Medium Viscosity Polyamide Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mix ratio 1 to 1 by weight.Tiga 291 EX Grey is a medium viscosity polyamide/ epoxy adhesive recommended for bonding applications where high shock impact resistance and peel resistance are desired. This 1 to 1 ratio, two-part adhesive is easily mixed and cured at room temperature and develops tough, strong bonds to a wide variety of materials including metals, glass, ceramics and plastics. Fully cured Tiga 291 EX Grey bonds offer superior thermal shock resistance, mechanical, electrical and impact resistant properties and low permeability to gases and vapors. The cured material has good dimensional stability and resistance to water, weather, oxygen and ozone, most petroleum products, mild acids and alkalis and many other chemicals.Applications: This system is recommended for low-stress, high impact/high peel strength bonding applications of dissimilar materials. Some proven applications are repairing strain gages, sealing seams on fiberglass components, repair of printed circuits, bonding stainless inserts inside potentiometers, bonding glass to aluminum, bonding of Pyrex, wire to Lucite, rubber hose to steel tubing, metal to fiberglass, repairing plastic laminates and sealing polyurethane foam.Information provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Of hardener
1.34 g/cc
1.34 g/cc
Of resin
Viscosity Measurement 40000

@Temperature 25.0 °C
40000

@Temperature 77.0 °F
Of hardener, RVT #7 @ 10 rpm
50000

@Temperature 25.0 °C
50000

@Temperature 77.0 °F
Mixed
60000

@Temperature 25.0 °C
60000

@Temperature 77.0 °F
Of resin, RVT #7 @ 10 rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
Thermal Properties Metric English Comments
CTE, linear 58.0 µm/m-°C

@Temperature 20.0 °C
32.2 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
2880 min

@Temperature 25.0 °C
48.0 hour

@Temperature 77.0 °F
Pot Life 100 min

@Temperature 25.0 °C
100 min

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Grey