Material Notes:
Notes: The Specialty Compounding Division offers a proprietary line of cap-liner compounds designed for carbonated soft drinks. These are proven products that have been used commercially for several years. These compounds are available pre-colored or natural, and can be tailored to specific needs. Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Melt Flow 16.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength at Break 9.79 MPa
1420 psi
ASTM D638
Elongation at Break 750 %
750 %
ASTM D638
Tensile Modulus 0.00517 GPa
0.750 ksi
ASTM D638