Physical Properties Metric English Comments
Melt Flow 16.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Elexar® EL 1934E Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Melt Flow 16.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Elexar® EL 3954-50 Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Melt Flow 16.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Elexar® EL 3954-62 Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Melt Flow 16.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Elexar® EL 3954-45 Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Melt Flow 16.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2815C Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 16.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
16.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Sinpolene MBB1934 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Uses: Sheet Forms: Pellets Processing Method: Injection Molding; Sheet Extrusion..
Melt Flow 16.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® 95-T0769V-90NT Ethylene Vinyl Acetate Copolymer
Notes: The Specialty Compounding Division offers a proprietary line of cap-liner compounds designed for carbonated soft drinks. These are proven products that have been used commercially for several..
Melt Flow 16.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Telcar® TL-1137 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 16.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-2478H Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 16.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
16.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-2545A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 16.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Melt Flow 16.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-94-T0586C-113 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 16.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
16.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-2545A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 16.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
16.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Telcar® TL-8730R Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 16.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
16.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Abstron HI40H ABS Injection Molding Grade
Automotive applications -Medium Impact, Super High Rigidity, PaintableInformation provided by Bhansali
Melt Flow 16.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
16.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Abstron HI40H ABS Injection Molding Grade
Automotive applications -Medium Impact, Super High Rigidity, PaintableInformation provided by Bhansali