Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.80 MPa | 1420 psi | ASTM D412 |
LG Chemical KEYFLEX TO-1175A Thermoplastic Olefin for Extrusion, 75A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Tensile Strength at Break | 9.81 MPa | 1420 psi | ASTM D638 |
Lotte Chemical Titan TITANLENE® LDI300YY Low density polyethylene resin LDI300YY is a low density polyethylene resin for injection molding and is a barefoot grade. LDI300YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2.. |
|||
Tensile Strength at Break | 9.76 MPa | 1420 psi | ISO R 527 |
Stir SpA B 3050 ATC (PVC) Application: Molding for boot-legInformation provided by STIR SpA |
|||
Tensile Strength at Break | 9.79 MPa | 1420 psi | |
Shin-Etsu Silicones FEA-251U Fluorosilicone Elastomer ShinEtsu FEA251 U is one of a series of fluorosilicone compounds. It is designed to process well in molding applications. It can be blended with other members of the series for intermediate hardness.. |
|||
Tensile Strength at Break | 9.79 MPa | 1420 psi | ASTM D638 |
Teknor Apex Telcar® 95-T0769V-90NT Ethylene Vinyl Acetate Copolymer Notes: The Specialty Compounding Division offers a proprietary line of cap-liner compounds designed for carbonated soft drinks. These are proven products that have been used commercially for several.. |
|||
Tensile Strength at Break | 9.80 MPa | 1420 psi | ASTM D882-83 |
DuPont Elvax® 40L-03 Ethylene-Vinyl Acetate Copolymer Resin Elvax® 40L-03 is an ethylene-vinyl acetate copolymer that is useful in many wire and cable applications because of its excellent mechanical, thermal, and low-smoke properties. The melt index is ap.. |
|||
Tensile Strength at Break | 9.79 MPa @Thickness 1.91 mm |
1420 psi @Thickness 0.0750 in |
20 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1934F Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Connectors; Wire Jacketing Agency Ratings: UL 1581Forms: Pellets Processing Method: Extrusion; Injec.. |
|||
Tensile Strength at Break | 9.81 MPa | 1420 psi | JIS-K-6723 |
Denka REOMER G G3000 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Tensile Strength at Break | 9.81 MPa | 1420 psi | JIS-K-6723 |
Denka REOMER G G5048 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Tensile Strength at Break | 9.81 MPa | 1420 psi | JIS-K-6723 |
Denka REOMER G G8250 Thermoplastic Elastomer, For Injection Molding Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Tensile Strength at Break | 9.79 MPa | 1420 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Tensile Strength at Break | 9.79 MPa | 1420 psi | |
Aearo E-A-R Specialty Composites Isoloss® HD Polyurethane Elastomer Isoloss® Polyurethane Elastomers feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protect.. |
|||
Tensile Strength at Break | 9.79 MPa | 1420 psi | ISO 37 |
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 9.79 MPa | 1420 psi | ISO 37 |
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |