Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex TEKRON® 4300-B88 UV Grade Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name TEKRON®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex TEKRON® 4300-B88 UV Grade Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
+/- 0.02; ASTM D792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
24 hrs
0.018 cm/cm
0.018 in/in
24 hrs + 30 min. at 82°C
Melt Flow 8.7 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.7 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
15 second delay. +/-3; ASTM D2240
Tensile Strength, Yield 12.4 MPa
1800 psi
ASTM D412
Elongation at Break 700 %
700 %
ASTM D412
Elongation at Yield 29.5 %
29.5 %
ASTM D412
10 %

@Temperature -35.0 °C
10 %

@Temperature -31.0 °F
ASTM D412
100% Modulus 0.00593 GPa
0.860 ksi
ASTM D412
300% Modulus 0.00683 GPa
0.990 ksi
ASTM D412
Flexural Modulus 0.1029 GPa
14.93 ksi
ASTM D790
Tear Strength 9.82 kN/m
56.0 pli
Die C; ASTM D1004
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 47.0 °C
117 °F
Flame Spread 32.5 mm/min
1.28 in/min
Pass: Burn Rate- Max 100; FMVSS 302
Descriptive Properties Value Comments
Fogging 95.2, 6 hours at 90°C. (SAE-J1756)