Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.7 g/10 min | 8.7 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 9007 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 8.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Silon Taborex TA 2126 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD, TA 1109 HD. TA 2126 HD contains the cross-linking catalyst to complete together with the above-mentioned graft a .. |
|||
Melt Flow | 8.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex TEKRON® 4300-B88 2UV Grade Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Melt Flow | 8.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex TEKRON® 4300-B88 UV Grade Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Melt Flow | 8.7 g/10 min @Temperature 230 °C |
8.7 g/10 min @Temperature 446 °F |
ASTM D1238 |
Dow DX5E66 Polypropylene Resin DOW DX5E66 is intended for use in cast film processes.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Melt Flow | 8.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar. |
|||
Melt Flow | 8.7 g/10 min | 8.7 g/10 min | Condition S; ASTM D 1238 |
CPT C-Flex® R70-091 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Melt Flow | 8.7 g/10 min | 8.7 g/10 min | |
Asahi Kasei Tenac®-C LV450 Copolymer Polyacetal Resin Applications: Automotive: Gears, Slides, Switches, Guides Electrical and Industrial: Gears, Slides, Railings, CamsInformation provided by Asahi Kasei |
|||
Melt Flow | 8.7 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.7 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® KU1-1230* Polycarbonate ISO 7391-PC,EFL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 8.5 cm3/10 minFlame retardant16 mm Triple wall sheet/B1 classification (DIN 4102)Medium viscosityUV stabilizedExtrusionAs of 1 Sept.. |