Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 12.4 MPa | 1800 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable 3201-xx05D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable JJF102L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 12.4 MPa @Treatment Temp. 136 °C, Time 605000 sec |
1800 psi @Treatment Temp. 277 °F, Time 168 hour |
Aging |
S&E Specialty Polymers TufFill NH™ GTPO8290-36 TPO Application: A 105°C rated, Flexible, TPO based, Zero Halogen compound, exhibiting excellent processing characteristics with superior physical and low temperature propertiesInformation provided by .. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G90S White Perfluoroelastomer Perlast ® G90S is a White Perfluoroelastomer 86-95 °IRHD with excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and formulated .. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | |
Resinlab® CYNERGY CA6605 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | |
Resinlab® CYNERGY CA6704 Adhesive Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal .. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | at 100%; ASTM D412 |
EG100A Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 12.4 - 19.3 MPa | 1800 - 2800 psi | Average value: 18.0 MPa Grade Count:71 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | |
Resinlab® CYNERGY CA6603 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ASTM D638 |
Global TPE-LS85A Elastomer Grade Data provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ASTM D638 |
Multibase Multi-Flex® G 7940 TPE Styrene Ethylene Butylene Styrene Block Copolymer Features: Chemical Resistance, Good General PurposeOzone Resistant Thermal Stability, Good Forms:PelletsProcessing Method:Injection MoldingBlow MoldingExtrusion Uses: Automotive ApplicationsInfor.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ASTM D638 |
Spartech SP-1310 Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ASTM D412 |
Teknor Apex TEKRON® 4300-B88 2UV Grade Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ASTM D412 |
Teknor Apex TEKRON® 4300-B88 UV Grade Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ASTM D638 |
ExxonMobil LD 506.07 Compounding and molding resin Product Description: LD 506.07 is a high flow, LDPE homopolymer designed to provide good processability. It is suitable for use in making color concentrates and injection molded articles.Availabilit.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ASTM D638 |
ExxonMobil LD 637.LI Molding, Extrusion and Compounding Resin Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ASTM D638 |
ExxonMobil LL 6202.19 Injection Molding Resin Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ASTM D638 |
ExxonMobil LLDPE LL 6201.19 Linear Low Density Polyethylene Resin Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | Molded property |
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045 Polyethylene resin is a premier film resin for heavy duty applications. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. The regulation sh.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | Molded property |
Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045.02AC Polyethylene resin is a high stability blown film extrusion resin that provides excellent tear strength and outstanding toughness. It contains high level of slip additive and medi.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | Molded property |
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045A Polyethylene blown film extrusion resin is a premier film resin for heavy duty applications. It is utilized where improved thermal stability over a broader range of processing conditi.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | Molded property |
Dow DOWLEX™ 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056A Polyethylene is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer with improved thermal stability and is an outstanding choice for cr.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | Molded property |
Dow DOWLEX™ 2245A Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2245A Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245A resin is used where improved thermal stability over a broad range of processing conditions is nece.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ISO R 527-2 |
Arkema Group OREVAC® 18350P Grafted Maleic Anhydride Polyethylene OREVAC 18350P is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE and HDPE coating for steel pipeline. It is mainly used in pipe coating to have good adhesion pe.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ASTM D-638 |
Axiall 11701 Wire & Cable Flexible PVC Non-lead stabilized, matte finish extrusion compound recommended for speaker wire and other general purpose extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ASTM D-638 |
Axiall 8808 Moldings & Extrusions Flexible PVC 105°C rated flexible polyvinyl chloride compound formulated for UL94 V-2 in all colors. The compound is formulated for sunlight resistance.Information provided by Georgia GulfGeorgia Gulf became A.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | ASTM D-638 |
Axiall 19750 Wire & Cable Flexible PVC 105°C rated insulation recommended for SPT cord applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | TM R050-36 |
Resinlab® EP1300 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1300 Black (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and .. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | Molded property |
Dow LDPE 535I Low Density Polyethylene, Liner Grade DOW LDPE 535I resin is a barefoot general purpose liner resin with medium clarity for medium modulus packaging applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for.. |
|||
Tensile Strength, Yield | 12.4 MPa | 1800 psi | TM R050-36 |
Resinlab® EP1305LV Black Epoxy Casting Resin Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |