Teknor Apex Laripur® LPR 9060HFM Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Teknor Apex Company
Trade Name Laripur®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Laripur® LPR 9060HFM Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: - Excellent performance under extreme and aggressive environments - Superior abrasion and cut resistance - Resistance to chemical, microbial attack and hydrolysis - Excellent flexibility at low temperatures - Good weathering properties - Non-halogen flame retardant - Low GlossApplications: - Energy & Power Cables: coiled or spiral: Construction / Mining - Automotive Cables: Anti-lock Braking Systems – ABS - Industrial Cables: Traffic / Signal / Trains / Boats / Buildings - Geophysical Cables: Land & Off-shore; Marine, Sub-sea & Umbilical - Telecommunications Cables: Telephone & Data Transmission; Military and Fiber Optics - Audio and Medical CablesInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
ASTM D2240
Tensile Strength 34.0 MPa
4930 psi
ASTM D412
Tensile Strength, Yield 7.412 MPa

@Strain 50.0 %
1075 psi

@Strain 50.0 %
ASTM D412
9.687 MPa

@Strain 100 %
1405 psi

@Strain 100 %
ASTM D412
13.00 MPa

@Strain 300 %
1885 psi

@Strain 300 %
ASTM D412
Elongation at Break 615 %
615 %
ASTM D412
Tear Strength 348 kN/m
1990 pli
ASTM D624
Thermal Properties Metric English Comments
Vicat Softening Point 83.9 °C
183 °F
ASTM D1525
Flammability, UL94 V-0

@Thickness 1.00 mm
V-0

@Thickness 0.0394 in
V-0

@Thickness 2.00 mm
V-0

@Thickness 0.0787 in
V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Descriptive Properties Value Comments
Abrasion Loss (mm3) 50
DIN 53516