Material Notes:
Type SI-RIG Silica Rigidizer is a single part water based colloidal suspension of colloidal silica. It is principally used for rigidizing and hardening the surfaces of ZIRCAR® fibrous ceramic products, but is also widely used as a coating agent and binder. Information provided by Zircar Ceramics.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
Particle Size 0.020 µm
0.020 µm
pH 9.3
9.3
Specific Surface Area 150 m²/g
150 m²/g
Viscosity Measurement 20

@Temperature 25.0 °C
20

@Temperature 77.0 °F
no units given
Component Elements Properties Metric English Comments
Na2O 0.080 %
0.080 %
SiO2 40 %
40 %
Descriptive Properties Value Comments
Color White
Stabilizing Ion Ammonium
Surface Charge Negative