Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 7.412 MPa @Strain 100 % |
1075 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Laripur® LPR 8860EG Thermoplastic Polyurethane Features: - Excellent performance under extreme and aggressive environments
- Superior abrasion and cut resistance
- Resistance to chemical, microbial attack and hydrolysis
- Excellent flexibility a.. |
|||
Tensile Strength, Yield | 7.412 MPa @Strain 50.0 % |
1075 psi @Strain 50.0 % |
ASTM D412 |
Teknor Apex Laripur® LPR 9060HFM Thermoplastic Polyurethane Features: - Excellent performance under extreme and aggressive environments
- Superior abrasion and cut resistance
- Resistance to chemical, microbial attack and hydrolysis
- Excellent flexibility a.. |