Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Flexalloy® 3500-40 Polyvinyl Chloride Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Vinyl (PVC)
Manufacturer Teknor Apex Company
Trade Name Flexalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Flexalloy® 3500-40 Polyvinyl Chloride Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
15 seconds; ASTM D2240
Tensile Strength, Yield 2.07 MPa
300 psi
100%; ASTM D412
6.96 MPa
1010 psi
ASTM D412
Elongation at Break 370 %
370 %
ASTM D412
Tear Strength, Total 510.6 N
114.8 lb (f)
Die C; ASTM D1004
Compression Set 12 %
12 %
73°F, 22 hr.; ASTM D395
57 %
57 %
158°F, 22 hr.; ASTM D395
70 %
70 %
212°F, 22 hr.; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -57.0 °C
-70.6 °F
ASTM D746