Polymer Property : Tensile Strength, Yield = 1010 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.96 MPa
1010 psi
ASTM D412
Polymax® Maxelast® A9735C TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Strength, Yield 6.96 MPa
1010 psi
ASTM D412
Polymax® Maxelast® P1985T TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 6.96 MPa
1010 psi
ASTM D412
Polymax® Maxelast® P3775H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 6.96 MPa
1010 psi
ASTM D412
Polymax® Maxelast® P3956 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 6.96 MPa
1010 psi
-13% change after 672 hours @ 200°C; ASTM D412
Precision Polymer Engineering S50R Silicone Rubber
Red Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain.Applications: Excellent heat resistance and low temperature flexibility. Used..
Tensile Strength, Yield 6.96 MPa
1010 psi
-13% change after 672 hours @ 200°C; ASTM D412
Precision Polymer Engineering S60R Silicone Rubber
Red Silicone 55-65 °IRHD. Diesel cylinder liner ring grade. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excell..
Tensile Strength, Yield 6.96 MPa
1010 psi
ASTM D412
Polymax® Maxelast® D6965H TPE, Extruded
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from..
Tensile Strength, Yield 6.96 MPa
1010 psi
ASTM D412
Teknor Apex Flexalloy® 3500-40 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te..
Tensile Strength, Yield 6.96 MPa
1010 psi
ASTM D412
Teknor Apex Flexalloy® 9900-40 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and ..
Tensile Strength, Yield 6.96 MPa

@Temperature 204 °C
1010 psi

@Temperature 400 °F
Flatwise Tensile; Composite Honeycomb Sandwich Performance; ASTM C 297
Hexcel® Redux® HP655 Toughened BMI film Adhesive
Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655..
Tensile Strength, Yield 6.98 MPa
1010 psi
cured 72 hrs @ RT
ACC QM 262F QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material
QM 262F is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin..