Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.96 MPa | 1010 psi | ASTM D412 |
Polymax® Maxelast® A9735C TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 6.96 MPa | 1010 psi | ASTM D412 |
Polymax® Maxelast® P1985T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 6.96 MPa | 1010 psi | ASTM D412 |
Polymax® Maxelast® P3775H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 6.96 MPa | 1010 psi | ASTM D412 |
Polymax® Maxelast® P3956 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 6.96 MPa | 1010 psi | -13% change after 672 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering S50R Silicone Rubber Red Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain.Applications: Excellent heat resistance and low temperature flexibility. Used.. |
|||
Tensile Strength, Yield | 6.96 MPa | 1010 psi | -13% change after 672 hours @ 200°C; ASTM D412 |
Precision Polymer Engineering S60R Silicone Rubber Red Silicone 55-65 °IRHD. Diesel cylinder liner ring grade. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excell.. |
|||
Tensile Strength, Yield | 6.96 MPa | 1010 psi | ASTM D412 |
Polymax® Maxelast® D6965H TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Strength, Yield | 6.96 MPa | 1010 psi | ASTM D412 |
Teknor Apex Flexalloy® 3500-40 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Tensile Strength, Yield | 6.96 MPa | 1010 psi | ASTM D412 |
Teknor Apex Flexalloy® 9900-40 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and .. |
|||
Tensile Strength, Yield | 6.96 MPa @Temperature 204 °C |
1010 psi @Temperature 400 °F |
Flatwise Tensile; Composite Honeycomb Sandwich Performance; ASTM C 297 |
Hexcel® Redux® HP655 Toughened BMI film Adhesive Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655.. |