Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.20e+13 ohm-cm | 1.20e+13 ohm-cm | ASTM D247 |
Plenco 2369 Phenolic, Granular, Injection Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Volume Resistivity | 1.20e+13 ohm-cm | 1.20e+13 ohm-cm | ASTM D257 |
Toyobo PELPRENE™ P80C Polyester TPE, High Flexibility, High Melting Point Features: Polyester TPE, High Flexibility, High Melting PointInformation provided by Toyobo. |
|||
Volume Resistivity | 1.20e+13 ohm-cm | 1.20e+13 ohm-cm | IEC 60093 |
DSM Arnitel® EM630 63 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Volume Resistivity | 1.20e+13 ohm-cm | 1.20e+13 ohm-cm | IEC 60093 |
DSM Arnitel® EM630 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Volume Resistivity | 1.20e+13 ohm-cm | 1.20e+13 ohm-cm | IEC 60093 |
DSM Arnitel® EM630-H Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Volume Resistivity | 1.20e+13 ohm-cm @Temperature 50.0 °C |
1.20e+13 ohm-cm @Temperature 122 °F |
ASTM D257 |
Teknor Apex APEX® 84132 Polyvinyl Chloride, Flexible Notes: 80°C Insulation and Jacketing; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Volume Resistivity | 1.20e+13 ohm-cm | 1.20e+13 ohm-cm | |
3M Scotch-Weld™ 3501 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 3501 B/A Gray is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume ar.. |
|||
Volume Resistivity | 1.20e+13 ohm-cm | 1.20e+13 ohm-cm | |
3M Scotch-Weld™ DP 3501 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP 3501 is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume are easi.. |