Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill FR® TPX-PBT-01006 40% Glass/Ceramic Filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Manufacturer Techmer ES
Trade Name HiFill FR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill FR® TPX-PBT-01006 40% Glass/Ceramic Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Ceramic, 40% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength 121 MPa
17500 psi
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 9.31 GPa
1350 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 18.0 µm/m-°C
10.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
ASTM D257
Dielectric Strength 18.1 kV/mm
460 kV/in
Method A (Short-Time); ASTM D149