Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® Naxel™ B720 Polycarbonate/PBT Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Nylene®
Trade Name Naxel™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® Naxel™ B720 Polycarbonate/PBT Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Naxel™ B720 is a Polycarbonate/PBT alloy. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 49.6 MPa
7200 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 1.72 GPa
250 ksi
ASTM D790
Izod Impact, Notched 9.61 J/cm
18.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C
145 °F
ASTM D648