Techmer ES HiFill FR® PA4/6 GF15 FR HS L 15% Glass Filled (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Flame Retarded + Glass Fiber Reinforced , Nylon 46, Lubricated + Glass Fiber Reinforced
Manufacturer Techmer ES
Trade Name HiFill FR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill FR® PA4/6 GF15 FR HS L 15% Glass Filled (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Water Absorption 2.0 %

@Time 86400 sec
2.0 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0075 cm/cm

@Thickness 3.17 mm
0.0075 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 82.7 MPa
12000 psi
ASTM D638
Elongation at Break 5.5 %
5.5 %
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm

@Thickness 3.17 mm
1.80 ft-lb/in

@Thickness 0.125 in
ASTM D256