Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan PU Corporation PPG CPU-1060 Polyurethane Casting Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer Taiwan PU Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation PPG CPU-1060 Polyurethane Casting Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, curing, demolding and after curing.Information provided by Taiwan PU Corporation.
Physical Properties Metric English Comments
Viscosity 1500 - 4000 cP

@Temperature 40.0 °C
1500 - 4000 cP

@Temperature 104 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
Tensile Strength at Break 2.94 - 6.86 MPa
426 - 995 psi
Elongation at Break 400 - 500 %
400 - 500 %
Tear Strength 19.6 - 58.8 kN/m
112 - 336 pli
Processing Properties Metric English Comments
Processing Temperature 100 °C
212 °F
Working Temperature, Prepolymer
Mold Temperature 100 °C
212 °F
Pot Life 30 min
30 min
Descriptive Properties Value Comments
MOCA Temperature 110°C
NCO Content Max 2.4%
Min 2.2%
PHR of MOCA 7%