TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Friction Compound

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Friction Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subjected to high wear in service. It has a unique combination of excellent properties, such as low temperature characteristics, and resistance to heat deterioration, ozone cracking, weathering and swelling in oils or solvents.The construction of an all-MILLATHANE CM unit is often desirable —for example, in the case of conveyor belts or other fabric inserted items. Better over-all abrasion resistance is thus obtained and the extra solvent wiping or cementing procedures required to satisfactorily bond MILLATHANE CM to other elastomers often can be eliminated.FormulationMillathane CM 100.0MT Carbon Black20.0Polyisobutylene Tackifier20.0Coumarone-Indene Resin20.0Sulfur0.75MBTS4.0MBT1.0CAYTUR 40.7Zinc Stearate0.5All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Tensile Strength, Yield 20.3 MPa
2950 psi
Elongation at Break 600 %
600 %
100% Modulus 0.00110 GPa
0.160 ksi
300% Modulus 0.00293 GPa
0.425 ksi
Tear Strength 26.2 kN/m
149 pli
Die C; ASTM D624
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 142 °C
1.00 hour

@Temperature 287 °F