Material Notes:
Finaclear® 530 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles, when used in blends with other styrenic polymers such as GPPS. Complemented by inherent reprocessing and recycling capability, Finaclear® 530 is a well established material in both food and non-food transparent packaging applications. Finaclear® 530 complies with most of the food regulations in European countries and with the Food and Drug Administration (FDA) in the USA.ApplicationFinaclear® 530 is designed for mono- and multilayer sheet extrusion/thermoforming, cast and blown film extrusion. Due to its specific structure and the well balanced styrene/butadiene ratio, Finaclear® 530 is the material of choice to reach and optimal balance between high impact, good clarity, brilliancy and cost.Information provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Bulk Density 0.620 g/cc
0.0224 lb/in³
ASTM D1895B
Density 1.02 g/cc
0.0368 lb/in³
Finaprene 2602 Method
Melt Index of Compound 11 g/10 min

@Load 5.00 kg,
Temperature 200 °C
11 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238G
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 25.0 MPa
3630 psi
ASTM D638
Elongation at Break <= 200 %
<= 200 %
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
ASTM D790
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
ASTM D256A
0.240 J/cm

@Temperature -30.0 °C
0.450 ft-lb/in

@Temperature -22.0 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C
153 °F
120°C/h; ASTM D648
Vicat Softening Point 82.0 °C
180 °F
ASTM D1252
Optical Properties Metric English Comments
Haze 3.0 %
3.0 %
ASTM D1003
Transmission, Visible 91 %
91 %
ASTM D1003