Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 95A

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 95A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed for applications in shoe soling, roll coverings and all other applications where transparent, brightly colored or decorative products are desired.FormulationMillathane 97 100Stearic Acid0.5Wacker HDK-N2030TP-95 (DBEEA)2Silquest A-1721.5Irganox 10100.25SR-231 (DEGDMA)20SR-350 (TMPTMA)20AC617A Polyethylene2Carbowax 33502Di-Cup R1All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
Tensile Strength, Yield 17.0 MPa
2470 psi
Elongation at Yield 160 %
160 %
100% Modulus 0.0128 GPa
1.85 ksi
Tear Strength 31.2 kN/m
178 pli
Die C
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 160 °C
0.167 hour

@Temperature 320 °F
Users viewing this material also viewed the following: