Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 95A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
100% Modulus | 0.0128 GPa | 1.86 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 3145D Thermoplastic Elastomer A high hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3145D can be processed by injection blow molding, molding or .. |
|||
100% Modulus | 0.0128 GPa | 1.86 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 3445D Thermoplastic Elastomer A NSF certified, high hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inje.. |
|||
100% Modulus | 0.0128 GPa | 1.86 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 3445DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
100% Modulus | 0.0128 GPa | 1.86 ksi | DIN 53504 |
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.0128 GPa | 1.85 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 95A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
100% Modulus | 0.0128 GPa | 1.85 ksi | ASTM D-638 |
Axiall 11890 Wire & Cable Flexible PVC High gloss, flame retardant jacketing compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0128 GPa | 1.85 ksi | ASTM D-638 |
Axiall 14880 Wire & Cable Flexible PVC 14880 is a non-lead stabilized, 80°C rated jacket with UL recognition for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20.. |
|||
100% Modulus | 0.0128 GPa | 1.85 ksi | ASTM D-638 |
Axiall 19930 Wire & Cable Flexible PVC THHN-THWN circuit sizes. Best suited for 105°C; 1/64 (18 AWG and larger). Rated VW-1. CSA approved TWN75, TEW, AWM IA, FT1 constructions. UL recognized for TW, THW, THWN, THHN. Oil resistant I.. |
|||
100% Modulus | 0.0128 - 0.0152 GPa | 1.85 - 2.20 ksi | Secant; Conditioned 7 days at RT/50% RH; ASTM D638 |
AdvanSource Biomaterials ChronoFlex® C 55D Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |
|||
100% Modulus | 0.0128 GPa | 1.85 ksi | ASTM D-638 |
Axiall 16901 Wire & Cable Flexible PVC 90°C rated fiber optic riser jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |