Material Notes:
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.Tribological and mechanical properties:Medium toughnessGood lubrication propertiesAdvantages and applications: Low friction coefficientLow wear of the counterpart Good transfer-film formationHigh electrical conductivity Suitable for pitch-bonded and resin-bonded brushes Fe-self lubricating engineering parts Fe-friction parts Copper/bronze bearings Copper friction parts copper clutch facingsInformation provided by TIMCAL
Physical Properties Metric English Comments
Bulk Density 0.240 g/cc
0.00867 lb/in³
Scott
Particle Size 5.0 µm
5.0 µm
Springback 11.5%, pressure 0.477 t/cc
20 µm
20 µm
Springback 13%, pressure 0.477 t/cc
23.1 µm
23.1 µm
d50
55.8 µm
55.8 µm
d90
48 - 65 µm
48 - 65 µm
d90, Guaranteed
75 µm
75 µm
Springback 17%, pressure 0.477 t/cc
550 µm
550 µm
at a density of 2.16 g/cc
1000 µm
1000 µm
at a density of 2.12 g/cc
Deformation 1.4 %
1.4 %
plastic
1.4 %
1.4 %
elastic
2.8 %
2.8 %
plastic + elastic
Ash 0.070 %
0.070 %
Typical
<= 0.10 %
<= 0.10 %
Guaranteed
Mechanical Properties Metric English Comments
Coefficient of Friction 0.30

@Temperature 850 °C,
Time 10800 sec
0.30

@Temperature 1560 °F,
Time 3.00 hour
Friction coefficient of sintered Cu-C -brake pads with 10% TIMREX® KS Graphite as a function of the particle size, Sinterdensity: 55% of the theoret. density
Thermal Properties Metric English Comments
Thermal Conductivity 140 W/m-K
972 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 1.55 ohm-cm
1.55 ohm-cm
particle size 80 um, pressure 2.5 t/cc
1.60 ohm-cm
1.60 ohm-cm
particle size 42 um, pressure 2.5 t/cc
1.80 ohm-cm
1.80 ohm-cm
particle size 15 um, pressure 2.5 t/cc
2.25 ohm-cm
2.25 ohm-cm
particle size 10 um, pressure 2.5 t/cc
Processing Properties Metric English Comments
Moisture Content 0.10 %
0.10 %
Typical
<= 0.50 %
<= 0.50 %
Guaranteed
Descriptive Properties Value Comments
Crystallite Height >100 nm
DBP absorption 98 g/100g
(Dibutylphthalate)
Users viewing this material also viewed the following: