Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Particle Size = 48 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 48 - 62 µm
48 - 62 µm
90%
H.C. Starck Amperit® 539.054 Agglomerated, Sintered Tungsten Carbide-Tungsten Boride-Cobalt-Chromium (WC-WB-Co-Cr) 60-30-5-5
Particle Size 48 - 58 µm
48 - 58 µm
90%
H.C. Starck Amperit® 553.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr)
Particle Size 48 µm
48 µm
d90
TIMCAL TIMREX® KC44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 48 - 65 µm
48 - 65 µm
d90, Guaranteed
TIMCAL TIMREX® KS75 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 48 µm
48 µm
90th%
3M S60HS Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Particle Size 48 - 52 µm
48 - 52 µm
Average; ATO 40-41-0 (Coulter Counter)
Arkema Group ORGASOL® 2002 ES 5 Nat 3 Polyamide 12
Information provided by Arkema Group
Copyright © lookpolymers.com All Rights Reserved