Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | <= 75 µm | <= 75 µm | VSD Powder |
Ferro CF 7555 Low-Temperature Sealing VITREOUS Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific .. |
|||
Particle Size | <= 75 µm | <= 75 µm | |
Ferro CF 7583 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific t.. |
|||
Particle Size | <= 75 µm | <= 75 µm | |
Ferro CF 7586 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific t.. |
|||
Particle Size | <= 75 µm | <= 75 µm | |
Ferro EG 2000 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |
|||
Particle Size | <= 75 µm | <= 75 µm | |
Ferro EG 2018 Display Device Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and .. |
|||
Particle Size | <= 75 µm | <= 75 µm | |
Ferro EG 4000 Display Device Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and .. |
|||
Particle Size | <= 75 µm | <= 75 µm | REG Powder |
Ferro IP 750 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | <= 75 µm | <= 75 µm | TF Powder |
Ferro IP 750 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | <= 75 µm | <= 75 µm | TF Powder |
Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | <= 75 µm | <= 75 µm | TF Powder |
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 75 µm | 75 µm | Maximum of 5% greater than |
H.C. Starck Amperit® 109.063 Agglomerated Sintered Molybdenum (Mo) |
|||
Particle Size | 75 µm | 75 µm | Maximum of 5% greater than |
H.C. Starck Amperit® 599.063 Agglomerated Sintered Molybdenum Carbide (Cr2O3) |
|||
Particle Size | 75 µm | 75 µm | Maximum of 2% greater than |
H.C. Starck Amperit® 821.084 Zirconia-Yttria 80-20 (ZrO2-Y2O3) |
|||
Particle Size | 75 - 100 µm | 75 - 100 µm | |
Lucite International Colacryl ® DP300U Specialty Acrylic Resin Colacryl® DP 300U has been designed for use as a dental polymer. Typical applications for this product include formulated, acrylic tooth polymer for manufacture of artificial teeth and denture ba.. |
|||
Particle Size | 75 - 105 µm | 75 - 105 µm | |
Lucite International Lucite® 41 Acrylic Resin for Casting and Embedments Lucite® 41 is a high molecular weight methyl methacrylate homopolymer for use in castings & embedments.Like all Lucite® Acrylic Resins for castings & embedments, Lucite® 41 offers: Exceptio.. |
|||
Particle Size | <= 75 µm | <= 75 µm | |
Ferro EG 2004 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |
|||
Particle Size | <= 75 µm | <= 75 µm | REG Powder |
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | <= 75 µm | <= 75 µm | REG Powder |
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | <= 75 µm | <= 75 µm | TF Powder |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | <= 75 µm | <= 75 µm | <5%; TI-2087 |
Solvay RHODOPOL® G Surfactant Description: Rhodopol® G is granular and dust free grade of Xanthan Gum. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing agent. It has rapid hydration propertie.. |
|||
Particle Size | 75 µm | 75 µm | Springback 17%, pressure 0.477 t/cc |
TIMCAL TIMREX® KS44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | Springback 17%, pressure 0.477 t/cc |
TIMCAL TIMREX® KS5-25 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | >= 75 µm | >= 75 µm | d50, 50%, vibrated sieving |
TIMCAL TIMREX® M100 mesh FR Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 75 µm | 75 µm | Springback 6.5%, pressure 0.477 t/cc |
TIMCAL TIMREX® SFG44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | at a density of 2.03 g/cc, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | springback 23%, pressure at 0.0477t/gg |
TIMCAL TIMREX® T75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 75 µm | 75 µm | at a density of 2.03 g/cc, pressure 2.5 t/cc |
TIMCAL TIMREX® SFG15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | <= 75 µm | <= 75 µm | < 3.0 wt% above |
Excalibar NewBar™ API Barite BaSO4 Powder NewBar™ API barite product is manufactured from a high-quality natural barium sulfate ore. Strict quality control results in a consistent product that is used in all phases of oil and gas explorati.. |
|||
Particle Size | 75 µm | 75 µm | 90th% |
3M S38 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | <= 75 µm | <= 75 µm | VSD Powder |
Ferro CF 7572 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet speci.. |