Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 2.25 ohm-cm | 2.25 ohm-cm | particle size 10 um, pressure 2.5 t/cc |
TIMCAL TIMREX® KS15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 2.25 ohm-cm | 2.25 ohm-cm | particle size 10 um, pressure 2.5 t/cc |
TIMCAL TIMREX® KS150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 2.25 ohm-cm | 2.25 ohm-cm | particle size 10 um, pressure 2.5 t/cc |
TIMCAL TIMREX® KS44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 2.25 ohm-cm | 2.25 ohm-cm | particle size 10 um, pressure 2.5 t/cc |
TIMCAL TIMREX® KS5-25 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 2.25 ohm-cm | 2.25 ohm-cm | particle size 10 um, pressure 2.5 t/cc |
TIMCAL TIMREX® KS5-44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 2.25 ohm-cm | 2.25 ohm-cm | particle size 10 um, pressure 2.5 t/cc |
TIMCAL TIMREX® KS5-75TT Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 2.25 ohm-cm | 2.25 ohm-cm | particle size 10 um, pressure 2.5 t/cc |
TIMCAL TIMREX® KS75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 2.25 ohm-cm | 2.25 ohm-cm | particle size 40 um, pressure 2.5 t/cc |
TIMCAL TIMREX® T150 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 2.25 ohm-cm | 2.25 ohm-cm | particle size 40 um, pressure at 2.5 t/cc |
TIMCAL TIMREX® T15-75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 2.25 ohm-cm | 2.25 ohm-cm | particle size 40 um, pressure of 2.5 t/cc |
TIMCAL TIMREX® T44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Electrical Resistivity | 2.25 ohm-cm | 2.25 ohm-cm | particle size at 40 um, pressure at 2.5 t/cc |
TIMCAL TIMREX® T75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |