Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 48 - 62 µm | 48 - 62 µm | 90% |
H.C. Starck Amperit® 539.054 Agglomerated, Sintered Tungsten Carbide-Tungsten Boride-Cobalt-Chromium (WC-WB-Co-Cr) 60-30-5-5 |
|||
Particle Size | 48 - 58 µm | 48 - 58 µm | 90% |
H.C. Starck Amperit® 553.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 48 µm | 48 µm | d90 |
TIMCAL TIMREX® KC44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 48 - 65 µm | 48 - 65 µm | d90, Guaranteed |
TIMCAL TIMREX® KS75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 48 µm | 48 µm | 90th% |
3M S60HS Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 48 - 52 µm | 48 - 52 µm | Average; ATO 40-41-0 (Coulter Counter) |
Arkema Group ORGASOL® 2002 ES 5 Nat 3 Polyamide 12 Information provided by Arkema Group |