Styron INSPIREâ„¢ TF1302 Thermoplastic Polyolefin

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Styron
Trade Name INSPIRE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron INSPIREâ„¢ TF1302 Thermoplastic Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792B
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638; ISO 527-2
Elongation at Yield 6.0 %
6.0 %
ASTM D638; ISO 527-2
Flexural Modulus 1.21 GPa
175 ksi
ASTM D709A
Izod Impact, Notched NB
NB
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C
200 °F
unannealed; ASTM D648; ISO 75-2/B