Styron CALIBREâ„¢ 701 15 Polycarbonate, General Purpose

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer Styron
Trade Name CALIBRE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron CALIBREâ„¢ 701 15 Polycarbonate, General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CALIBRE® 701 series polycarbonate resins are a general purpose, transparent, ignition resistant grades equipped with a mold release package. The CALIBRE 701 series resins exhibit a high heat resistance, high clarity and are rated V-0 at 3.2 mm according to UL-94(1).The CALIBRE 701 resins are typically used in applications like electrical components and in building and construction areas due to the increasing ignition resistance requirements.Available Melt Flow Rate: 15.(1) These numerical flame spread ratings are small scale test values and are not intended to reflect hazards presented by these or any other materials under actual fire conditions.Ignition resistant chemical additives increase resistance to burning from minor flame sources and permit properly manufactured end products to meet the requirements of certain flammability tests, but resins will burn rapidly under the right conditions of heat and oxygen feed.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM Data
Water Absorption 0.15 %
0.15 %
Moisture Absorption at Equilibrium 0.32 %
0.32 %
Humidity Absorption
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Melt Flow 15 g/10 min

@Load 1.20 kg,
Temperature 300 °C
15 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM Data
Mechanical Properties Metric English Comments
Hardness, Rockwell R 123
123
Tensile Strength, Ultimate 65.5 MPa
9500 psi
ASTM Data
Tensile Strength, Yield 60.7 MPa
8800 psi
ASTM Data
Elongation at Break 120 %
120 %
ASTM Data
Tensile Modulus 2.24 GPa
325 ksi
ASTM Data
Izod Impact, Notched 8.54 J/cm
16.0 ft-lb/in
ASTM Data
Izod Impact, Unnotched NB
NB
ASTM Data
Tensile Impact Strength 462 kJ/m²
220 ft-lb/in²
ASTM Data
Impact Test 79.1 J

@Temperature 23.0 °C
58.3 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM data
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
261 °F
Unannealed; ASTM Data
Vicat Softening Point 154 °C
309 °F
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Oxygen Index 41 %
41 %
Optical Properties Metric English Comments
Haze 1.1 %
1.1 %
Transmission, Visible 86 %
86 %