Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Impact Strength = 462 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 462 kJ/m²
220 ft-lb/in²
ASTM Data
Styron CALIBREâ„¢ 200 15 Polycarbonate, General Purpose
CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins ..
Tensile Impact Strength 462 kJ/m²
220 ft-lb/in²
ASTM D1822
Styron CALIBREâ„¢ 200-14 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-14 polycarbonate resin is a natural, FDA compliant, 14 melt flow rate general purpose polycarbonate resin with no mold release or UV stabilizer.Govt. and Industry Standar..
Tensile Impact Strength 462 kJ/m²
220 ft-lb/in²
ASTM D1822
Styron CALIBREâ„¢ 201-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-15 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
Tensile Impact Strength 462 kJ/m²
220 ft-lb/in²
ASTM Data
Styron CALIBREâ„¢ 2060 15 Polycarbonate, Sterilization Grade
CALIBRE® 2060 series resins are designed for those applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clari..
Tensile Impact Strength 462 kJ/m²
220 ft-lb/in²
ASTM Data
Styron CALIBREâ„¢ 2071 15 Polycarbonate, Sterilization Grade
CALIBRE® 2071 resins are designed for those applications which use steam or ethylene oxide for sterilization while providing enhanced mold release characteristics. This material has excellent ret..
Tensile Impact Strength 462 kJ/m²
220 ft-lb/in²
ASTM Data
Styron CALIBREâ„¢ 300 15 Polycarbonate, General Purpose
CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren..
Tensile Impact Strength 462 kJ/m²
220 ft-lb/in²
ASTM D1822, Type S
Styron CALIBREâ„¢ 301-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Impact Strength 462 kJ/m²
220 ft-lb/in²
ASTM Data
Styron CALIBREâ„¢ 701 15 Polycarbonate, General Purpose
CALIBRE® 701 series polycarbonate resins are a general purpose, transparent, ignition resistant grades equipped with a mold release package. The CALIBRE 701 series resins exhibit a high heat resi..
Tensile Impact Strength 462 kJ/m²
220 ft-lb/in²
ASTM D1822, Type S
Styron CALIBREâ„¢ 201-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Impact Strength 462 kJ/m²
220 ft-lb/in²
ASTM D1822, Type S
Styron CALIBREâ„¢ 303-15 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Impact Strength 462 kJ/m²
220 ft-lb/in²
Molded and tested per ASTM D4976; ASTM D1822, Type S
Dow UNIVAL™ DMDA-6147 NT 7 High Density Polyethylene Resin (HDPE)
Good extrudability/processability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6147 NT 7 is a polymer with broad molecular weight distribution and high molecular weight. This produ..