Polymer Property : Impact Test = 79.1 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 79.1 J

@Temperature 23.0 °C
58.3 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Styron CALIBREâ„¢ 701 15 Polycarbonate, General Purpose
CALIBRE® 701 series polycarbonate resins are a general purpose, transparent, ignition resistant grades equipped with a mold release package. The CALIBRE 701 series resins exhibit a high heat resi..